Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Meforex® 142b Ozone-Friendly CFC Replacement

Category Fluid
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name Meforex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Meforex® 142b Ozone-Friendly CFC Replacement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formula: CH3CClF2; Name: 1,1,1 Chlorodifluoroethane. Replaces CFC 11, 12, 114. Polyethylene and polystyrene foams, and heat pumps.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc

@Temperature 25.0 °C
0.0405 lb/in³

@Temperature 77.0 °F
Liquid
Molecular Weight 100.5 g/mol
100.5 g/mol
Vapor Pressure 3.38 bar

@Temperature 25.0 °C
2540 torr

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 214.5 J/g
92.28 BTU/lb
at Boiling Point
Melting Point -131.1 °C
-204.0 °F
at 1.013 bar
Boiling Point -9.20 °C
15.4 °F
at 1.013 bar
Chemical Properties Metric English Comments
Critical Pressure 42.5 bar
31900 torr
Critical Temperature 137.1 °C
278.8 °F
Critical Density 0.430 g/cc
0.0155 lb/in³
Descriptive Properties Value Comments
Flammability Range (vol%) 9.0 to 14.8
Users viewing this material also viewed the following: