Thermal Properties Metric English Comments
Melting Point -131.1 °C
-204.0 °F
at 1.013 bar
Solvay Specialty Polymers Meforex® 142b Ozone-Friendly CFC Replacement
Formula: CH3CClF2; Name: 1,1,1 Chlorodifluoroethane. Replaces CFC 11, 12, 114. Polyethylene and polystyrene foams, and heat pumps.Information provided by Solvay Solexis, Inc.