Material Notes:
Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ASTM D891
Viscosity Measurement 343
343
Viscosity Index; ASTM D2270
Kinematic Viscosity 550 cSt

@Temperature 20.0 °C
550 cSt

@Temperature 68.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 310 cSt
310 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 86 cSt
86 cSt
ASTM D445
Molecular Weight 12500 g/mol
12500 g/mol
Evaporation Loss 0.40 %
0.40 %
22 hrs. at 204°C; ASTM 2595
Surface Tension 25 dynes/cm
25 dynes/cm
ASTM D1331
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 112 kg
247 lb (mass)
Mean Hertz Load; IP 239
500 kg
1100 lb (mass)
Init. Seiz. Load; IP 239
708 kg
1560 lb (mass)
Welding Load; IP 239
Four Ball Wear 1.21 mm

@Load 40.0 kg,
Temperature 75.0 °C
0.0476 in

@Load 88.2 lb,
Temperature 167 °F
Avg. scar diameter; 1200 RPM, 60 min; ASTM D4172 B
Thermal Properties Metric English Comments
Pour Point -60.0 °C
-76.0 °F
ASTM D97