Physical Properties Metric English Comments
Molecular Weight 12500 g/mol
12500 g/mol
Solvay Specialty Polymers FOMBLIN® M100 PFPE Lubricant
Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc.
Molecular Weight 12500 g/mol
12500 g/mol
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant
Information provided by Solvay Solexis, Inc.