Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 550 cSt @Temperature 20.0 °C |
550 cSt @Temperature 68.0 °F |
ASTM D445 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |