Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 708 kg | 1560 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Four Ball Extreme Pressure, Weld Load | 708 kg | 1560 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Four Ball Extreme Pressure, Weld Load | 708 kg | 1560 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® YR PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Four Ball Extreme Pressure, Weld Load | 708 kg | 1560 lb (mass) | Welding Load; IP 239 |
Solvay Specialty Polymers FOMBLIN® W800 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |