Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of thermal expansion, which means excellent dimensional stability. Creep resistance is also exceptional. This grade has been approved for use with potable water in the United States, France, Germany, and the United Kingdom. - Natural: A-1145 NT DW - Black: A-1145 BK 937 DWInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183/A
Filler Content 45 %
45 %
Glass Fiber Reinforcement
Mechanical Properties Metric English Comments
Tensile Strength, Yield 232 MPa
33600 psi
ISO 527-2
Elongation at Break 1.8 %

@Temperature 23.0 °C
1.8 %

@Temperature 73.4 °F
ISO 527-2
Tensile Modulus 15.1 GPa
2190 ksi
ISO 527-2
Flexural Strength 330 MPa
47900 psi
ISO 178
Flexural Modulus 14.0 GPa

@Temperature 23.0 °C
2030 ksi

@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO) 7.80 kJ/m²
3.71 ft-lb/in²
ISO 180
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 302 °C
576 °F
Unannealed; ISO 75-2/Af
Processing Properties Metric English Comments
Rear Barrel Temperature 316 - 329 °C
601 - 624 °F
Middle Barrel Temperature 316 - 329 °C
601 - 624 °F
Front Barrel Temperature 324 - 335 °C
615 - 635 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 150 °C
302 °F
Drying Temperature 120 °C
248 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content 0.030 - 0.060 %
0.030 - 0.060 %
Descriptive Properties Value Comments
Agency Ratings NSF 61
Tested at 82 °C (180 °F) (Commercial Hot)
Appearance Black
Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Chlorine Resistant
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Stiffness
High Stiffness
High Strength
High Temperature Strength
Low Moisture Absorption
Forms Pellets
Generic PPA
Processing Method Injection Molding
RoHS Compliance RoHS Compliant
Uses Appliances
Consumer Applications
Filters
Housings
Industrial Applications
Plumbing Parts
Pump Parts
Valves/Valve Parts
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved