Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:.. |
|||
Front Barrel Temperature | 324 - 340 °C | 615 - 644 °F | |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Front Barrel Temperature | 324 °C | 615 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Front Barrel Temperature | 324 - 340 °C | 615 - 644 °F | |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Front Barrel Temperature | 324 - 340 °C | 615 - 644 °F | |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Front Barrel Temperature | 324 °C | 615 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Front Barrel Temperature | 324 °C | 615 °F | |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Front Barrel Temperature | 324 - 345 °C | 615 - 653 °F | |
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-8950 HS Polyphthalamide (PPA), 50% Glass Fiber Amodel® A-8950 HS is a 50% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance, low mo.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® DW-1150 Polyphthalamide (PPA)
(Unverified Data**) Amodel DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of th.. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of .. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers. |
|||
Front Barrel Temperature | 324 - 335 °C | 615 - 635 °F | |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |