Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Algoflon® 0.1 Mos PTFE; Molybdenum Disulfide Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® 0.1 Mos PTFE; Molybdenum Disulfide Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.0.1 wt.% Molybdenum Disulfide. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost no moisture absorption, low friction coefficient, and is nonflammable.
Physical Properties Metric English Comments
Density 2.17 g/cc
0.0784 lb/in³
ASTM D792
Apparent Bulk Density 0.450 g/cc
0.0163 lb/in³
ASTM D4894
Linear Mold Shrinkage 0.033 cm/cm
0.033 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
Tensile Strength, Ultimate 38.0 MPa
5510 psi
ASTM D638
Elongation at Break 370 %
370 %
ASTM D638
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Coefficient of Friction, Static 0.080
0.080
ASTM D1894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service