Physical Properties Metric English Comments
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Nabaltec NABALOX® NO 615-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Nabaltec NABALOX® NO 625-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Nabaltec NH 20 Aluminum Hydroxide
Used in the production of glass and ceramic productsaluminum fluoride, cryolite and other aluminum saltsfrits and pigmentsmolecular sievescatalystsrefractory productspigments
Bulk Density 0.500 - 1.20 g/cc
0.0181 - 0.0434 lb/in³
Apparent Density
Indium Corp. Standard ITO Indium Tin Oxide
Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo..
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Inhance Fluoro-Seal INHANCE® Ti-9000 Titanium Carbide
Product Description: INHANCE Ti-9000 consists of spherically shaped titanium carbide micro grains. This product is used to make other INHANCE polymer alloys. When incorporated in polymers, unique ..
Bulk Density 1.10 - 1.20 g/cc
0.0397 - 0.0434 lb/in³
Inhance Fluoro-Seal INHANCE® Ti-9100 Titanium Carbide Polymer Alloy
Product Description: INHANCE Ti-9100 polymer alloy consists of spherically shaped titanium carbide micro grains coated with a thin layer of a proprietary coupling agent. This product was designed ..
Bulk Density 0.500 - 1.20 g/cc
0.0181 - 0.0434 lb/in³
Apparent Density
Indium Corp. Fine ITO Indium Tin Oxide
Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo..
Bulk Density 0.600 - 1.20 g/cc
0.0217 - 0.0434 lb/in³
Solvay Chemicals NOCOLOK® Zn Flux
Reactive flux alternative to arc spray Zn coating.HS No.: 38109090 /CAS-No.: 13827-02-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical ..
Bulk Density 0.900 - 1.20 g/cc
0.0325 - 0.0434 lb/in³
Solvay Chemicals Oxyper® S131 Sodium Percarbonate
Oxyper® S131 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products and environmental applications; it may be suitabl..
Bulk Density 0.900 - 1.20 g/cc
0.0325 - 0.0434 lb/in³
Solvay Chemicals Oxyper® S142 Sodium Percarbonate
Oxyper® S142 is a stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in formulated bleach additive products, detergent powders and tablets, automa..
Bulk Density 0.900 - 1.20 g/cc
0.0325 - 0.0434 lb/in³
Solvay Chemicals Oxyper® SHC Sodium Percarbonate
Oxyper® SHC is a high coated, stabilized grade of sodium percarbonate (Sodium carbonate peroxyhydrate) specially designed for use in bleach additive products, detergent powders and tablets, autom..
Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
540MA3C63
Solvay MIRAPOL® SURF-S 411 HA Surfactant
Description: Rinse aid polymer specially formulated for auto dish wash powders and tablets. Recommended as a substitute to rinse aid surfactants. Enables raw material cost saving, while boosting rin..
Bulk Density 0.800 - 1.20 g/cc
0.0289 - 0.0434 lb/in³
Solvay Chemicals (CsAlF-Complex) Cesium Fluoroaluminate
Low-melting-point flux for brazing aluminum.HS No.: 38109090 /CAS-No.: 138577-01-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appl..