Solvay IGEPAL® CA 520 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name IGEPAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay IGEPAL® CA 520 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: ETHOXYLATED OCTYLPHENOLCAS: 9002-93-1; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CA-520 is an excellent solubilizer for hair dye formulations. IGEPAL© CA-520 is used in the applications for: pesticide and floor polish emulsifier and for non-polar hydrocarbon solvents, inexpensive automotive anti-icing additive, paper and pulp formulations, industrial metal cleaner, and dry cleaning detergents.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Molecular Weight 426 g/mol
426 g/mol
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to Slightly Hazy Liquid
RP-0064
Color <160
APHA, RP-0134
HLB number 10
Hydroxyl Number 126-136 mg KOH/g
RP-0245
Ionic Charge Nonionic
Neutralization Number <0.5 mg KOH/g
pH7, RP-0343