Polymer Property : Molecular Weight = 426 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 426 g/mol
426 g/mol
Theoretical
PolyOne Synplast™ DIDA-E Di Isodecyl Adipate
Branched C10 adipate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne
Molecular Weight 426 g/mol
426 g/mol
Solvay IGEPAL® CA 520 Surfactant
Chemical Name: ETHOXYLATED OCTYLPHENOLCAS: 9002-93-1; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CA-520 is an excellent solubilizer for hai..