Material Notes:
Description: Liquid Sodium Methyl Cocoyl Taurate that demonstrates good lathering properties in skin cleanser and shampoo applications. Displaysexcellent dispersiblity properties in hard water and high electrolyte loadsChemical Name: SODIUM N-COCONUT ACID-N-METHYL TAURATE CAS: 61791-42-2; 61788-47-4; 7732-18-5Biodegradability: Readily biodegradable, Closed Bottle >80% in 28 daysAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: GEROPON® TC-42 LQ is a liquid anionic surfactant with excellent solubility and outstanding detergency and wetting properties coupled with dispersing and suspending action. It is stable in high electrolyte systems, mild acids and is mild to hair and skin. GEROPON® TC-42 LQ exhibits excellent lathering properties similar to fatty acid soaps. Unlike soaps, GEROPON® TC-42 LQ is stable in mildly acidic systems and displays good performance properties in hard water solutions.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Volatiles 70 %
70 %
by Volume
pH 6.0 - 7.0
6.0 - 7.0
as is @25°C; RP-0420
Thermal Properties Metric English Comments
Flash Point >= 93.0 °C
>= 199 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear to Cloudy Liquid
May Precipitate Upon Storage, RP0064
Color <200
APHA, RP-0134
Composition Active
33-36%, EQ. WT. 363, RP-0027
Free Fatty Acid
<5.0%, RP-0971
Odor Typical Fatty