Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name Trimid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120.1 MPa
17420 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Yield Strength 164.8 MPa
23900 psi
ASTM D790
Flexural Modulus 4.56 GPa
661 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm

@Thickness 3.17 mm
1.29 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature <= 216 °C
<= 420 °F
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Front Barrel Temperature 238 - 266 °C
460 - 510 °F
Nozzle Temperature 238 - 266 °C
460 - 510 °F
Melt Temperature 232 - 271 °C
450 - 520 °F
Mold Temperature 21.1 - 93.3 °C
70.0 - 200 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 - 4 hour
3 - 4 hour
Injection Pressure 82.7 - 172 MPa
12000 - 25000 psi
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Screw Speed 40 - 80 rpm
40 - 80 rpm