Material Notes:
Made by suspension polymerisation. APPLICATIONS Filler polymer for plastisols - Floor covering : hard-wearing top coats, chemically blown and mechanical foams, impregnation layers - Wall coverings - Artificial leathers - Tarpaulins - Undersealing compounds for motor vehicles - Seals for bottle caps. CHARACTERISTICS SolVin 266SF filler polymer is a suspension resin with very low porosity and small particle size. Used in formulations for plastisols up to 50 phr, it lowers viscosity and substantially reduces ageing of the paste during storage. It can also appreciably reduce the cost of the formulation. SPECIAL PROPERTIES The addition of SolVin 266SF : - permits, holding viscosity constant, a reduction in plasticisation or an increase in mineral filler content - reduces considerably the process of viscosity increase during storage - eliminates the tendency to dilatancy observed with some resins used in low-plasticized formulations which leads to difficult-to-process pastes (e.g. SolVin 372LD) - alters only very slightly the gelation properties and the capacity to form chemically-blown foams - permits adjustment of the mattness and surface feel of a gelled plastisol - permits preparation of pastes with a wide non-sticking temperature range.Information provided by SolVin.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content <= 0.30 g/l
<= 0.30 g/l
ISO 1269
Apparent Bulk Density >= 0.780 g/cc
>= 0.0282 lb/in³
Compacted; ISO 1068
Particle Size 45 µm
45 µm
average; ISO 1624
90 µm
90 µm
<0.5 g/kg greater than value; ISO 1624
125 µm
125 µm
<0.05 g/kg greater than value; ISO 1624
Viscosity Test 109 cm³/g
109 cm³/g
Reduced viscosity, K value = 66; ISO 1628-2