Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 109 - 136 cm³/g | 109 - 136 cm³/g | Average value: 124 cm³/g Grade Count:4 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Viscosity Test | 109 cm³/g | 109 cm³/g | Reduced viscosity, K value = 66; ISO 1628-2 |
SolVin 266SF Polyvinyl Chloride Pastes - filler Polymers Made by suspension polymerisation.
APPLICATIONS
Filler polymer for plastisols
- Floor covering : hard-wearing top coats, chemically blown and mechanical foams, impregnation layers
- Wall coverings
-.. |