Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.529 - 0.593 g/cc | 0.0191 - 0.0214 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Bulk Density | 0.529 g/cc | 0.0191 lb/in³ | As Supplied |
Skamol Group Skamol M-20 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |