Silikony Polskie Gumosil M Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Silikony Polskie
Trade Name Gumosil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Gumosil M Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexible with good tearing resistance
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Before Curing
Viscosity 45000 cP
45000 cP
Before Curing
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
After Curing
Mechanical Properties Metric English Comments
Hardness, Shore A 21
21
After Curing
Tensile Strength at Break 4.70 MPa
682 psi
After Curing
Elongation at Break 600 %
600 %
After Curing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Processing Properties Metric English Comments
Cure Time <= 1440 min
<= 24.0 hour
Curing
Pot Life 90 - 120 min
90 - 120 min
Curing
Descriptive Properties Value Comments
Color White