Sichuan Deyang Haton® 1.8 dtex Polyphenylene Sulfide Staple Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Sichuan Deyang Chemical Co. Ltd.
Trade Name Haton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sichuan Deyang Haton® 1.8 dtex Polyphenylene Sulfide Staple Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD
Physical Properties Metric English Comments
Fiber Count 1.80 dtex
1.62 denier
GB/T14335-2008
Mechanical Properties Metric English Comments
Elongation at Break 53 %
53 %
GB/T1040.2-2006
Tenacity 0.440 N/tex
4.99 g/denier
GB/T14337-2008
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 170 °C
338 °F
Oxygen Index 40 %
40 %
GB/T5454-1997
Descriptive Properties Value Comments
Length, mm 51
Linear Density, dtex 1.8
GB/T14335-2008