Solvay MIRATAINE® H-30 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MIRATAINE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MIRATAINE® H-30 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mirataine H-30 is a high foaming betaine surfactant that demonstrates excellent stability properties over broad pH ranges. Typically used as a secondary surfactant in anionic based systems, Mirataine H-30 improves overall foam quality and also helps improve formulation mildness.Chemical Name: ALKYL C12-C14 BETAINESCAS: 683-10-3; 2601-33-4Compatibility: All surfactant classesUse level: 1-10%Available in: North AmericaApplications: MIRATAINE ® H-30 is a high foaming betaine surfactant that demonstrates excellent stability properties over broad pH ranges. Typically used as a secondary surfactant in anionic based systems, MIRATAINE ® H-30 improves overall foam quality and also helps improve formulation mildness.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
5% Solution; RP-0420
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 5.0 ppm
<= 5.0 ppm
RP-0277
Processing Properties Metric English Comments
Moisture Content 60 - 64 %
60 - 64 %
100 Solid; RP-0536
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Alkalinity 1.15-1.30 meq/g
RP-17117
Appearance Clear Pale Yellow Liquid
RP-0064
Color <100
APHA, RP-0134
Composition Active
29-31%, MW 279, RP-1438
Free Alkldimethylamine in Betaines
<0.5%, RP-17512
SMCA
<100 ppm, As is Basis, RP-0108
Sodium Chloride
6.5-7.5%, RP-0097