Goodfellow Copper 90/Titanium 10 Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Copper 90/Titanium 10 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1000 °C
1830 °F
Component Elements Properties Metric English Comments
Copper, Cu 90 %
90 %
Titanium, Ti 10 %
10 %