Shinil Chemical SHINCON PA66 Electro Conductive Polymer

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Shinil Chemical
Trade Name SHINCON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINCON PA66 Electro Conductive Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.Feature and BenefitsPermanent electro conductivityMaintain the physical properties of base resinNo particulates (CNT product)Lighter weightRecyclabilityEasy processingImproved surfaceCost effectiveGrade/Application: EMI shieldingInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 216 MPa
31300 psi
Flexural Strength 372.78 MPa
54067 psi
Flexural Modulus 22.8 GPa
3300 ksi
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.040 ohm-cm
0.040 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Users viewing this material also viewed the following: