Material Notes:
Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
Viscosity 600000 cP
600000 cP
B
650000 cP
650000 cP
A
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 22
22
Tensile Strength 5.70 MPa
827 psi
Elongation at Yield 870 %
870 %
100% Modulus 0.000359 GPa
0.0520 ksi
Tear Strength 36.0 kN/m
205 pli
Compression Set 15 %

@Temperature 150 °C,
Time 3600 sec
15 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 26
T10 (302°F, ODR)
38
T90 (302°F, ODR)
Users viewing this material also viewed the following: