Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 600000 - 800000 cP @Temperature 25.0 °C |
600000 - 800000 cP @Temperature 77.0 °F |
Uncured |
Permabond ES578 Epoxy Resin PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon.. |
|||
Viscosity | 600000 - 600000 cP @Temperature 420 - 420 °C |
600000 - 600000 cP @Temperature 788 - 788 °F |
Average value: 600000 cP Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Viscosity | 600000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
600000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Viscosity | 600000 cP @Temperature 420 °C |
600000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Viscosity | 600000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
600000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Viscosity | 600000 cP | 600000 cP | Melt Viscosity; SABIC Method |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Viscosity | 600000 cP | 600000 cP | Melt Viscosity; SABIC Method |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Viscosity | 600000 cP | 600000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 600000 cP | 600000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 600000 cP | 600000 cP | B |
Shin-Etsu Silicones LIMSâ„¢ KE2090-70AB Elastomer KE-2090-70 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Viscosity | 600000 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
600000 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Viscosity | 600000 cP @Temperature 180 °C |
600000 cP @Temperature 356 °F |
Melt; Flowtester (100 kgf/cm², dimension of die 1 Φ mm x 10 mm) |
Zeon Chemicals Quintac® 3620 SIS Block Polymer Styrene Isoprene (SIS) Block Polymer. Standard grade for hot melt PSAInformation provided by Zeon Chemicals L.P. |
|||
Viscosity | 600000 cP | 600000 cP | |
Loctite® PST® 580 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Viscosity | 600000 cP @Shear Rate 0.100 1/s, Temperature 280 °C |
600000 cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
DSM Akulon® F130-E5 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock |
|||
Viscosity | 600000 cP @Temperature 160 °C |
600000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 600000 cP @Temperature 160 °C |
600000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 2A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 600000 cP | 600000 cP | Dynamic |
Dow Corning 1418 Fluid A blend of an ultrahigh viscosity polydimethicone in an intermediate viscosity dimethicone for use in skincare, suncare, hair care, color cosmetic, and an antiperspirnt/deodorant applications.Inform.. |
|||
Viscosity | 600000 - 1.50e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
600000 - 1.50e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 2501-20 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Very flexible, very soluble. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low p.. |