Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name Sharada
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc

@Temperature 200 °C
0.0145 lb/in³

@Temperature 392 °F
Mechanical Properties Metric English Comments
Compressive Strength 0.392 MPa

@Temperature 800 °C
56.9 psi

@Temperature 1470 °F
Cold Crushing
0.883 MPa

@Temperature 200 °C
128 psi

@Temperature 392 °F
Cold Crushing
0.981 MPa

@Temperature 1200 °C
142 psi

@Temperature 2190 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 0.139 W/m-K

@Temperature 500 °C
0.965 BTU-in/hr-ft²-°F

@Temperature 932 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
Component Elements Properties Metric English Comments
Al2O3 25 %
25 %
Fe2O3 1.5 %
1.5 %
Processing Properties Metric English Comments
Moisture Content 70 - 80 %
70 - 80 %
Recommended