Polymer Property : Compressive Strength = 0.392 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 0.392 MPa

@Temperature 800 °C
56.9 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 7 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 0.392 MPa

@Temperature 800 °C
56.9 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 0.392 MPa

@Temperature 800 °C
56.9 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.5 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 0.392 - 1.37 MPa

@Temperature 110 °C,
Time 86400 sec
56.9 - 199 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-80S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 0.392 - 1.37 MPa

@Temperature 500 °C,
Time 10800 sec
56.9 - 199 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-80S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).