Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.883 MPa @Temperature 200 °C |
128 psi @Temperature 392 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 0.883 MPa @Temperature 200 °C |
128 psi @Temperature 392 °F |
Cold Crushing |
Sharadaa Ceramics Sharada LTM 0.5 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |