Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shandong Dongyue Shenzhou New Material Co DS2603 Fluoroelastomer Copolymer Gum

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co DS2603 Fluoroelastomer Copolymer Gum.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulcanizing process, FKM products have excellent mechanical performance, outstanding anti oil property (fuel oil, synthesis oil, lubricating oil) and high thermal stability.Main Applications:Widely used in high temperature, aviation, automobile, petroleum and chemical industries, oils, lubricants, etc. Mainly used to produce gaskets, O-rings, V-rings, sealing bowl with metal bone, diaphragms, tube, valve-plate, rolls, etc.Properties: Middle and high viscosity, good milling and calendaring performanceApplication: Calendaring sheet, skeletal oil seal, extruded hose etc.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.80 - 1.84 g/cc
1.80 - 1.84 g/cc
Mooney Viscosity 61 - 79

@Temperature 121 °C
61 - 79

@Temperature 250 °F
ML(1+10); DS2603-1
80 - 100

@Temperature 121 °C
80 - 100

@Temperature 250 °F
ML(1+10); DS2603-2
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 11.5 MPa
>= 1670 psi
>= 9.50 MPa

@Temperature 275 °C,
Time 86400 sec
>= 1380 psi

@Temperature 527 °F,
Time 24.0 hour
Elongation at Break >= 160 %
>= 160 %
>= 130 %

@Temperature 275 °C,
Time 86400 sec
>= 130 %

@Temperature 527 °F,
Time 24.0 hour
Compression Set <= 25 %

@Temperature 200 °C,
Time 86400 sec
<= 25 %

@Temperature 392 °F,
Time 24.0 hour
AF compression rate 30%
Descriptive Properties Value Comments
Appearance White or light yellow translucent rubber piece
Oil Resistance (%) <6
1# aircraft fuel, 200°C, 24h, added weight)