Mechanical Properties Metric English Comments
Tensile Strength at Break <= 9.50 MPa
<= 1380 psi
ISO/R527
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Tensile Strength at Break <= 9.50 MPa
<= 1380 psi
ISO/R527
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Tensile Strength at Break 9.51 MPa
1380 psi
ASTM D638
LG Chemical LC170 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Tensile Strength at Break >= 9.50 MPa

@Temperature 275 °C,
Time 86400 sec
>= 1380 psi

@Temperature 527 °F,
Time 24.0 hour
Shandong Dongyue Shenzhou New Material Co DS2603 Fluoroelastomer Copolymer Gum
Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc..
Tensile Strength at Break >= 9.50 MPa

@Temperature 275 °C,
Time 86400 sec
>= 1380 psi

@Temperature 527 °F,
Time 24.0 hour
Shandong Dongyue Shenzhou New Material Co DS2604 Fluoroelastomer Copolymer Gum
Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc..
Tensile Strength at Break 9.51 MPa
1380 psi
DCBP Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..
Tensile Strength at Break 9.51 MPa
1380 psi
DBPH Cure
Shin-Etsu Silicones SV-18000U Silicone Rubber
SV18000U is one of a series of easy processing, mineral filled silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering. Product Fe..
Tensile Strength at Break 9.50 MPa
1380 psi
ASTM D638
UBE J2522 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Tensile Strength at Break 9.51 MPa
1380 psi
Change in tensile strength after 18 hours at 250°F, in vegetable oil; ASTM D471
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Tensile Strength at Break 9.50 MPa
1380 psi
ISO 37
ELASTO UK Dryflex® 5064-101 TPE, Modified Injection Molding Grade for Auto Mud Flaps
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5064-101 is specifically designe..