Mechanical Properties Metric English Comments
Tensile Strength at Break 11.5 MPa
1670 psi
IEC 60811
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Tensile Strength at Break 11.5 MPa
1670 psi
200mm/min; ASTM D638
LG Chemical LUTENE LB7500 LDPE Extrusion Coating
Description: LUTENE LB7500 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB7500 is also noted for the excellent adhesion to porous a..
Tensile Strength at Break 11.5 MPa
1670 psi
ASTM D638
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol..
Tensile Strength at Break >= 11.5 MPa
>= 1670 psi
Shandong Dongyue Shenzhou New Material Co DS2603 Fluoroelastomer Copolymer Gum
Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc..
Tensile Strength at Break >= 11.5 MPa
>= 1670 psi
Shandong Dongyue Shenzhou New Material Co DS2604 Fluoroelastomer Copolymer Gum
Conformable with: Q/DYS 005-2007Brief Introduction:FKM-DS2600 is copolymer of HFP and VDF. Normally it is white or light yellow translucent elastomer whose fluorine content is over 66%. After vulc..
Tensile Strength at Break 11.5 MPa
1670 psi
ASTM D638
Teknor Apex APEX® 3700-65 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 11.5 MPa
1670 psi
ISO 527-2
Carmel Olefins IPETHENE® 830 Low Density Polyethylene
IPETHENE® 830 is a low density polyethylene injection molding grade. It exhibits high melt flow rate and high stiffness. APPLICATIONS IPETHENE® 830 is used to produce lids, containers, toys, and..