Physical Properties Metric English Comments
Density 2.43 g/cc
0.0878 lb/in³
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Density 2.43 g/cc
0.0878 lb/in³
Schott NG4 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG1, NG5, NG9, NG10, NG11, NG 12
Density 2.43 g/cc
0.0878 lb/in³
Schott NG5 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG1, NG9, NG10, NG11, NG 12
Density 2.43 g/cc
0.0878 lb/in³
UBE Tyranno Grade H Ceramic Semi-Conductive Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..
Density 2.43 g/cc
0.0878 lb/in³
UBE Tyranno Grade G Ceramic Semi-Conductive Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..