Material Notes:
General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 2.13 g/cc
0.0770 lb/in³
ASTM D792
Deformation 7.0 %

@Time 86400 sec
7.0 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength 20.7 MPa
3000 psi
ASTM D4894
Elongation at Break 200 %
200 %
ASTM D4894
Tensile Modulus 0.386 GPa
56.0 ksi
ASTM D4894
Compressive Yield Strength 13.1 MPa

@Strain 1.00 %
1900 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 0.758 GPa
110 ksi
ASTM D695
Coefficient of Friction 0.09
0.09
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature 26.0 - 200 °C
71.7 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 126 µm/m-°C

@Temperature 26.0 - 200 °C
70.0 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Descriptive Properties Value Comments
Color Dark Gray
Users viewing this material also viewed the following: