Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature 20.0 °C
71.7 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate  (discontinued **)
16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature -30.0 - 100 °C
71.7 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP
SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod..
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature 26.0 - 200 °C
71.7 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
Saint-Gobain Fluoroloy® A15 High Performance Seal Material
Improved sealing at low pressure; Can be abrasive running against soft metals Information provided by Saint-Gobain Performance Plastics.
CTE, linear, Parallel to Flow 129 µm/m-°C

@Temperature 26.0 - 200 °C
71.7 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
Saint-Gobain Fluoroloy® A16 High Performance Seal Material
General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service Information provided by Saint-Goba..