SSAB Tunnplat Domex® 500MC HSLA Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Domex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Domex® 500MC HSLA Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum Si content of 0.03% is not available, the silicon content should be 0.2%..Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel.Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 550 - 700 MPa
79800 - 102000 psi
Tensile Strength, Yield >= 500 MPa
>= 72500 psi
Elongation at Break >= 14 %

@Thickness >=3.00 mm
>= 14 %

@Thickness >=0.118 in
A<sub>80</sub>
>= 18 %

@Thickness >=3.00 mm
>= 18 %

@Thickness >=0.118 in
A<sub>5</sub>
Impact 168
168
J/cm²; -20°C
174

@Temperature -40.0 °C
174

@Temperature -40.0 °F
J/cm²
Bend Radius, Minimum >= 1.0 t
>= 1.0 t
t<3mm; internal bend radius, 90°
>= 1.2 t
>= 1.2 t
3 mm < t< 6mm; internal bend radius, 90°
>= 1.6 t
>= 1.6 t
t>6mm; internal bend radius, 90°
Component Elements Properties Metric English Comments
Aluminum, Al >= 0.015 %
>= 0.015 %
Carbon, C <= 0.10 %
<= 0.10 %
Iron, Fe 98 %
98 %
As remainder
Manganese, Mn <= 1.6 %
<= 1.6 %
Niobium, Nb (Columbium, Cb) <= 0.090 %
<= 0.090 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.30 %
<= 0.30 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti <= 0.15 %
<= 0.15 %
Vanadium, V <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: