Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Bend Radius, Minimum | >= 1.2 t | >= 1.2 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 500MC HSLA Steel HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum .. |
|||
Bend Radius, Minimum | >= 1.2 t | >= 1.2 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 550MC HSLA Steel HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n.. |
|||
Bend Radius, Minimum | >= 1.2 t | >= 1.2 t | 3 mm < t< 6mm; internal bend radius, 90° |
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |