Bend Radius, Minimum >= 1.2 t
>= 1.2 t
3 mm < t< 6mm; internal bend radius, 90°
SSAB Tunnplat Domex® 500MC HSLA Steel
HSLA SteelCharacteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum ..
Bend Radius, Minimum >= 1.2 t
>= 1.2 t
3 mm < t< 6mm; internal bend radius, 90°
SSAB Tunnplat Domex® 550MC HSLA Steel
HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n..
Bend Radius, Minimum >= 1.2 t
>= 1.2 t
3 mm < t< 6mm; internal bend radius, 90°
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..