Material Notes:
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron steels are used for a wide variety of applications - as a wear material and as a high-strength structural steel. Examples include wear plate, screen plate, punching tools, spades, knives, saw blades, caterpillar tracks, and agricultural machinery.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Hardness, Vickers 540
540
HV<sub>10</sub>; approximate
Tensile Strength, Ultimate 1720 MPa
249000 psi
Tensile Strength, Yield 1200 MPa
174000 psi
Elongation at Break 10 %
10 %
A<sub>5</sub>
Impact 15
15
J/cm²; -20°C
25
25
J/cm²; 20°C
Component Elements Properties Metric English Comments
Boron, B 0.0030 %
0.0030 %
Carbon, C 0.25 - 0.30 %
0.25 - 0.30 %
Chromium, Cr 0.15 - 0.25 %
0.15 - 0.25 %
Iron, Fe 98 %
98 %
As Remainder
Manganese, Mn 1.0 - 1.3 %
1.0 - 1.3 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.20 - 0.35 %
0.20 - 0.35 %
Sulfur, S <= 0.025 %
<= 0.025 %
Users viewing this material also viewed the following: