Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1200 - 1520 MPa | 174000 - 220000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Yield | 1200 MPa @Strain 0.200 % |
174000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
SSAB Tunnplat Domex® 014 BOR Water quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
SSAB Tunnplat Domex® 024 BOR Water quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
SSAB Tunnplat Domex® 034 BOR Water quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
SSAB Tunnplat Domex® 044 BOR Water quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
ThyssenKrupp XAR® 450 Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 450.Application: The steel may be used for wear exposed structures, e.g. excavati.. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | |
ThyssenKrupp XAR® PLUS Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® PLUS.Application: The steel may be used for wear exposed structures, e.g. excavat.. |
|||
Tensile Strength, Yield | 1200 MPa @Strain 0.200 % |
174000 psi @Strain 0.200 % |
Typical |
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila.. |
|||
Tensile Strength, Yield | 1200 MPa | 174000 psi | at HRC 45 |
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti.. |
|||
Tensile Strength, Yield | 1200 MPa @Temperature 100 °C |
174000 psi @Temperature 212 °F |
R<sub>p</sub>02. Short transverse direction. |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Tensile Strength, Yield | 1200 - 1500 MPa | 174000 - 218000 psi | |
ArcelorMittal MartINsite® 1500 Cold Rolled Steel Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me.. |
|||
Tensile Strength, Yield | 1200 MPa @Strain 0.200 % |
174000 psi @Strain 0.200 % |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Tensile Strength, Yield | 1200 - 1520 MPa | 174000 - 220000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its .. |