Polymer Property : Tensile Strength, Yield = 1200 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1200 - 1520 MPa
174000 - 220000 psi
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Yield 1200 MPa

@Strain 0.200 %
174000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 1200 MPa
174000 psi
SSAB Tunnplat Domex® 014 BOR Water quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1200 MPa
174000 psi
SSAB Tunnplat Domex® 024 BOR Water quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1200 MPa
174000 psi
SSAB Tunnplat Domex® 034 BOR Water quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1200 MPa
174000 psi
SSAB Tunnplat Domex® 044 BOR Water quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1200 MPa
174000 psi
ThyssenKrupp XAR® 450 Structural Steel
This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 450.Application: The steel may be used for wear exposed structures, e.g. excavati..
Tensile Strength, Yield 1200 MPa
174000 psi
ThyssenKrupp XAR® PLUS Structural Steel
This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® PLUS.Application: The steel may be used for wear exposed structures, e.g. excavat..
Tensile Strength, Yield 1200 MPa

@Strain 0.200 %
174000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 551 (Ti-4Al-4Mo-4Sn-0.5Si) Titanium Alloy; 25-100 mm
High-Strength Forging AlloyIndustry Specifications: UK Aerospace Specifications BS TA.38, 39, 40, 41, 42.Features: TIMETAL 551 has high strength and is creep resistant up to 400°C. It has a simila..
Tensile Strength, Yield 1200 MPa
174000 psi
at HRC 45
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel
Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti..
Tensile Strength, Yield 1200 MPa

@Temperature 100 °C
174000 psi

@Temperature 212 °F
R<sub>p</sub>02. Short transverse direction.
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Tensile Strength, Yield 1200 - 1500 MPa
174000 - 218000 psi
ArcelorMittal MartINsite® 1500 Cold Rolled Steel
Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me..
Tensile Strength, Yield 1200 MPa

@Strain 0.200 %
174000 psi

@Strain 0.200 %
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C
Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati..
Tensile Strength, Yield 1200 - 1520 MPa
174000 - 220000 psi
Materion Beryllium Copper Alloy 25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its ..
Copyright © lookpolymers.com All Rights Reserved