SSAB Tunnplat Domex® 024 BOR Water quenched Boron Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Domex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Domex® 024 BOR Water quenched Boron Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron steels are used for a wide variety of applications - as a wear material and as a high-strength structural steel. Examples include wear plate, screen plate, punching tools, spades, knives, saw blades, caterpillar tracks, and agricultural machinery.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Hardness, Vickers 490
490
HV<sub>10</sub>; approximate
Tensile Strength, Ultimate 1600 MPa
232000 psi
Tensile Strength, Yield 1200 MPa
174000 psi
Elongation at Break 10 %
10 %
A<sub>5</sub>
Impact 25
25
J/cm²; -20°C
35
35
J/cm²; 20°C
Component Elements Properties Metric English Comments
Boron, B 0.0030 %
0.0030 %
Carbon, C 0.20 - 0.25 %
0.20 - 0.25 %
Chromium, Cr 0.15 - 0.25 %
0.15 - 0.25 %
Iron, Fe 98 %
98 %
As Remainder
Manganese, Mn 1.0 - 1.3 %
1.0 - 1.3 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.20 - 0.35 %
0.20 - 0.35 %
Sulfur, S <= 0.025 %
<= 0.025 %