Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding of intricate parts. Typical applications are circuit breakers, insulators, bobbins and electrical connectors.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.85 - 2.05 g/cc
0.0668 - 0.0741 lb/in³
Molded
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
Tensile Strength 52.4 - 66.2 MPa
7600 - 9600 psi
Flexural Strength 103 - 131 MPa
15000 - 19000 psi
Flexural Modulus 7.58 - 8.96 GPa
1100 - 1300 ksi
Compressive Strength 124 - 152 MPa
18000 - 22000 psi
Izod Impact, Notched 3.04 - 4.11 J/cm
5.70 - 7.70 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 15.3 - 17.3 kV/mm
389 - 439 kV/in
short time
Arc Resistance >= 187 sec
>= 187 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F