Material Notes:
Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known for its capabilities in high-temperature environments and its chemical resistance, Greene, Tweed`s Fluoraz has proven field performance in both dynamic and static applications.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
After 70hrs @347°F in Stauffer 7700
90
90
ASTM D2240
Tensile Strength at Break 15.7 MPa
2280 psi
After 70hrs @347°F in Stauffer 7700
20.7 MPa
3000 psi
ASTM D1414
Tensile Strength, Yield 18.10 MPa
2625 psi
@100% Elongation; ASTM D1414
Elongation at Break 120 %
120 %
ASTM D1414
153.6 %
153.6 %
After 70hrs @347°F in Stauffer 7700
Compression Set 18 %
18 %
166 hours @ 347°F @ 25% deflection; ASTM D395
35 %
35 %
22 hours @ 392°F @ 25% deflection; ASTM D395
18 %

@Temperature 23.0 °C
18 %

@Temperature 73.4 °F
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -6.67 °C
20.0 °F
Shrinkage -18.0 %

@Temperature 175 °C,
Time 252000 sec
-18.0 %

@Temperature 347 °F,
Time 70.0 hour
in Stauffer 7700