Dow Corning EP-9293 AL Cosmetic Powder

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning EP-9293 AL Cosmetic Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A unique combination of a white cross-linked dimethyl polysiloxane elastomer powder and fumed alumina. As with EP-9289 LL, this combination allows the powder to improve flow and reduce agglomeration, providing superior handling ease. Additionally, the powder provides dual feel, soft focus properties, has good compaction properties when formulated into a pressed powder, a high sebum absorption profile and the ability to thicken volatile silicone.INCI Name: Dimethicone/Vinyl Dimethicone Crosspolymer (and) AluminaInformation provided by Dow Corning
Physical Properties Metric English Comments
Bulk Density 0.100 - 0.300 g/cc
0.00361 - 0.0108 lb/in³
Volatiles <= 1.0 %
<= 1.0 %
Particle Size 3.0 - 5.0 µm
3.0 - 5.0 µm
Processing Properties Metric English Comments
Shelf Life 27.0 Month
27.0 Month