Polymer Property : Izod Impact, Notched (ISO) = 54.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 54.0 kJ/m²

@Temperature 23.0 °C
25.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled
AS171L-02US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability.This product is available ..
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
ISO 180/1A
S&E Specialty Polymers TufFill™ 5008 Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CE3510 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact, high heat and excellent extrusion and thermoforming characteristics. Halogen free..
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS
Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® HP9NR PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding ..
Izod Impact, Notched (ISO) 54.0 kJ/m²

@Temperature -30.0 °C
25.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® ML7664 PC Copolymer (Asia Pacific)
Lexan* ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. Lexan* ML7664 resin is a non-FR product availabl..
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP NX07354 PC+ABS (Asia Pacific)
This is a PC/ABS compound, a good candidate for Laser Direct Structuring applications.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific)
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV00CES PA 66
LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific)
LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 54.0 kJ/m²
25.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RX06424 PA 66
LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural