Polymer Property : Flexural Modulus = 2.268 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.268 GPa
328.9 ksi
ISO 178
S&E Specialty Polymers TufFill™ 5008 Polyolefin
Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p..
Flexural Modulus 2.268 GPa
328.9 ksi
ISO 178
MRC Polymers NAXELLâ„¢ PC429MHI Polycarbonate, Impact Modified
• Medium MFR• Good property retention, heat and dimensional stability• Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants ca..