S&E Specialty Polymers GTPR-1358A

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer S&E Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers GTPR-1358A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Rubber material designed for winter boot applications requiring excellent abrasion and stitch tear.  Available in a wide range of colors.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.08 g/cc
1.02 - 1.08 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 51 - 57

@Time 15.0 sec
51 - 57

@Time 0.00417 hour
ASTM D2240
Tensile Strength 4.48 MPa
650 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Descriptive Properties Value Comments
Rossflex 0
Cut Growth @ 10,000 flexes
Users viewing this material also viewed the following: