Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D 792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
0.0080 - 0.010 cm/cm

@Thickness 6.40 mm
0.0080 - 0.010 in/in

@Thickness 0.252 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
SABIC - Japan Method
Elongation at Break 5.0 %
5.0 %
SABIC - Japan Method
Flexural Strength 147 MPa
21300 psi
ASTM D 790
Flexural Modulus 5.88 GPa
853 ksi
ASTM D 790
Izod Impact, Notched 0.590 J/cm

@Temperature 23.0 °C
1.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
UL 94
Users viewing this material also viewed the following: