Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL PX4716 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX4716 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS GF15% FR V-1
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.20 mm
0.0050 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 12.2 g/10 min

@Load 5.00 kg,
Temperature 300 °C
12.2 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 78.0 MPa
11300 psi
SABIC - Japan Method
Elongation at Break 5.0 %
5.0 %
SABIC - Japan Method
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 4.72 GPa
685 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm
2.21 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
25.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 134 °C

@Thickness 6.40 mm
273 °F

@Thickness 0.252 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in air; ASTM D149
Users viewing this material also viewed the following: