SABIC Innovative Plastics Lexan® ML6451 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® ML6451 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 10.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa
10400 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 71.0 MPa
10300 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 98 %
98 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 104 MPa
15100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 114 °C

@Thickness 3.20 mm
237 °F

@Thickness 0.126 in
unannealed; ASTM D648