Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 244RF PC (Asia Pacific) LEXAN 244RF resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ3420 PC Medium Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ3420 PC (Asia Pacific) Medium Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 141 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 141S PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 243 PC 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats.. |
|||
Melt Flow | 10.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
Granulate; ISO 1133/U |
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn.. |
|||
Melt Flow | 10.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 10.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 10.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
10.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Melt Flow | 10.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 901 MS POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 210 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Reliance Industries PVAXX H60 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
KKPC KOSYN KTR 302 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |